Warhammer 40k

It's plastic, not resin, right? You didn't get a Finecast or Russian special without realizing it, did you?
Inquisitor_BadAss

Warhammer 40k

Maybe the issue was that you layered the glue over itself? Try scraping the glue off, then give the contact area a light sanding. Once that’s done...
Meiwaku

Warhammer 40k

How humid is it where you live? Too humid can cause failure as the glue reacts to the atmosphere. Are the parts fully clean and free of debris and...
WhatInTheActualFuck

Warhammer 40k

Never, to be honest. That said, I don't layer the glue. For most well-fitting joints, I hold them together and apply the cement to the seam and...